    The experimental observations on ageing have been briefed. Thus, it seems that the degradation depends on the time and occurs most rapidly at temperatures of 200-300°C. Even it is caused by the tetragonal-monoclinic transformation, the phenomenon it is always accompanied by micro- and macro-cracking. The process develops from the exterior and continues inside the sample.… Continue reading Aging resistance upon on Bloomden 3D Pro multi-layer and other zirconia blocks